MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper-Cobalt-Beryllium alloy, UNS C17500, H04 Temper rod, bar, plate, tubing
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability.

Applications: fuse clips, fasteners, springs, switch and relay parts, electrical conductors, welding equipment.

H04 temper rod, bar, plate, or tubing.

Key Words: BeCu; low beryllium copper, C112, ISO CuCo2Be, CEN CW104C, A3/1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 60 - 8060 - 80Rod, bar, plate, tubing
Tensile Strength, Ultimate 450 - 550 MPa65300 - 79800 psiRod, bar, plate, tubing
Tensile Strength, Yield 380 - 515 MPa
@Strain 0.2 %
55100 - 74700 psi
@Strain 0.2 %
rod, bar, plate, tubing
Elongation at Break 10 - 15 %10 - 15 %In 50 mm, rod, bar, plate, tubing
Modulus of Elasticity 125 - 130 GPa18100 - 18900 ksi
Fatigue Strength 205 MPa29700 psiRod, bar, plate, tubing
Machinability 40 %40 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000057 - 0.0000086 ohm-cm
@Temperature 20.0 °C
0.0000057 - 0.0000086 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 200 °C
9.78 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 17.3 W/m-K120 BTU-in/hr-ft²-°F
Melting Point 1030 - 1070 °C1890 - 1960 °F
Solidus 1030 °C1890 °F
Liquidus 1070 °C1960 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 980 °C1800 °FHot-Shortness Temperature
Solution Temperature 900 - 925 °C1650 - 1700 °FLarge sections, 1 hour per inch or fraction of an inch
 900 - 955 °C1650 - 1750 °F10 minutes, water quench
Aging Temperature 425 °C797 °F3-6 hours, for maximum strength
 470 - 495 °C878 - 923 °FCommercial practice, 2-3 hours
Hot-Working Temperature 700 - 925 °C1290 - 1700 °F
Precipitation Temperature >= 482 °C
@Time 7200 sec
>= 900 °F
@Time 2.00 hour
Air
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.40 - 0.70 %0.40 - 0.70 %
Cobalt, Co 2.4 - 2.7 %2.4 - 2.7 %
Copper, Cu 96.9 %96.9 %
Iron, Fe >= 0.10 %>= 0.10 %
Other, total >= 0.50 %>= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper-Cobalt-Beryllium alloy, UNS C17500, TB00 Temper strip, rod, bar, plate, tubing, forged products
Copper-Cobalt-Beryllium alloy, UNS C17500, HTR (Proprietary mill hardening) Temper
Copper-Cobalt-Beryllium alloy, UNS C17500, TF00 Temper strip, rod, bar, plate, tubing, forged products
Copper-Cobalt-Beryllium alloy, UNS C17500, HTC (Proprietary mill hardening) Temper
Beryllium Copper, UNS C17200, TH04 Temper rod, bar, plate, tubing, >25 mm

MC17500b8 / 10901

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.