Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Applications: fuse clips, fasteners, springs, switch and relay parts, electrical conductors, welding equipment. H04 temper rod, bar, plate, or tubing. |
BeCu; low beryllium copper, C112, ISO CuCo2Be, CEN CW104C, A3/1 |