MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman BMC 501E Mineral Filled, Glass Reinforced Polyester
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame resistance, and low water absorption. Distinguished from other materials by its very soft flow, it is an excellent compound for encapsulating delicate components.

Typical applications include coil and solenoid Encapsulation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.77 g/cc1.77 g/cc
Water Absorption 0.10 %0.10 %24 hours, 23°C
Linear Mold Shrinkage 0.00 - 0.0015 cm/cm0.00 - 0.0015 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol <= 10<= 10
Tensile Strength, Ultimate 27.6 - 41.4 MPa4000 - 6000 psi
Flexural Strength 68.9 - 82.7 MPa10000 - 12000 psi
Compressive Strength 75.8 - 103 MPa11000 - 15000 psi
Izod Impact, Notched 0.801 - 1.60 J/cm1.50 - 3.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.9
@Frequency 60 Hz
4.9
@Frequency 60 Hz
Dielectric Strength 11.8 kV/mm300 kV/inShort Time
Dissipation Factor 0.0070
@Frequency 60 Hz
0.0070
@Frequency 60 Hz
Arc Resistance >= 180 sec>= 180 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C>= 400 °F
Flammability, UL94  V-0
@Thickness 6.35 mm
V-0
@Thickness 0.250 in
 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Mold Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 610 Mineral Filled, Glass Reinforced Polyester Compound
A. Schulman BMC 5209 Mineral Filled, Glass Reinforced Polyester
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Avient OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, PUR

PBMC062 / 27245

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.