Product Description: LExxonMobil™ C4LL 2018.YB is a C4 Ziegler Natta LLDPE for Low Voltage power cable and Telecom jacketing. The grade contains a higher level of antioxidants and has excellent Environmental Stress Crack Resistance (ESCR). Sufficient Carbon Black or UV stabilizer should be added to meet cable jacketing specifications. Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Halogen-free flame retardant (HFFR) compounds
- LV silane cross-linkable – 2 step process
- LV thermoplastic jacketing
- MV/HV thermoplastic jacketing
- Telecom thermoplastic jacketing
Information provided by ExxonMobil |
LLDPE LL 1002YB Wire & Cable |