MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: DOW DNDA-8320 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D792
ESCR 100% Igepal® 20 hour
@Temperature 50.0 °C
20 hour
@Temperature 122 °F
F50; Molded and tested in accordance with ASTM D4976; ASTM D1693
Melt Index of Compound 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 7.58 MPa1100 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 11.7 MPa1700 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 60 %60 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 3.0 %3.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 0.386 GPa
@Strain 2 %
56.0 ksi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength 168 kJ/m²80.0 ft-lb/in²Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FDow Method (DSC)
Crystallization Temperature 108 °C226 °FDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 42.8 °C109 °FMolded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 93.9 °C201 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FMolded and tested in accordance with ASTM D4976; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin
Dow GRSN-9820 NT 7 Linear Low Density Polyethylene Granular Solid
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade

PDOW1274 / 30492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.