MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Entec Hylex® P1010FR Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes:

Information provided by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Water Absorption 0.14 %0.14 %24 hrs; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D785
Tensile Strength at Break 65.5 MPa9500 psiASTM D638
Elongation at Break 120 %120 %ASTM D638
Flexural Strength 89.6 MPa13000 psiASTM D790
Flexural Modulus 2.14 GPa310 ksiASTM D790
Izod Impact, Notched 6.41 J/cm12.0 ft-lb/in73°F, 0.125 in; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+16 ohm-cm4.00e+16 ohm-cmASTM D257
Dielectric Strength 15.0 kV/mm380 kV/inin Air, 0.125 in; ASTM D149
Arc Resistance 90 sec90 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C290 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FUnannealed; ASTM D648
Vicat Softening Point 152 °C305 °FASTM D1525
Flammability, UL94 V-0
@Thickness 1.55 mm
V-0
@Thickness 0.0610 in
NA
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5851.585ASTM D542
Haze 0.90 - 1.0 %
@Thickness 3.17 mm
0.90 - 1.0 %
@Thickness 0.125 in
ASTM D1003
Transmission, Visible 87 - 89 %87 - 89 %125 mil; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 271 - 282 °C520 - 540 °F
Middle Barrel Temperature 277 - 288 °C530 - 550 °F
Front Barrel Temperature 282 - 299 °C540 - 570 °F
Nozzle Temperature 277 - 299 °C530 - 570 °F
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 76.7 - 93.3 °C170 - 200 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 12 hour3 - 12 hour
Moisture Content <= 0.020 %<= 0.020 %
Injection Pressure 6.89 - 12.4 MPa1000 - 1800 psi
Back Pressure 0.483 - 1.03 MPa70.0 - 150 psi
Shot Size 40 - 60 %40 - 60 %
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
Holding Pressure700 to 1200 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Entec Hylex® P1010L1 HB Polycarbonate
Ravago Manufacturing Americas Hylex® P1010G10 HB Polycarbonate, 10% Fiberglass Reinforced
Ravago Manufacturing Americas Hylex® P1310G15 HB Polycarbonate, 15% Fiberglass Reinforced, UV Stabilized
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized

PENTA034 / 36044

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.