MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Entec Hylex® P1010FR Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes:

Information provided by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.14 %24 hrs; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Tensile Strength at Break 9500 psiASTM D638
Elongation at Break 120 %ASTM D638
Flexural Strength 13000 psiASTM D790
Flexural Modulus 310000 psiASTM D790
Izod Impact, Notched 12.0 ft-lb/in73°F, 0.125 in; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+16 ohm-cmASTM D257
Dielectric Strength 380 V/milin Air, 0.125 in; ASTM D149
Arc Resistance 90 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 290 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 275 °FUnannealed; ASTM D648
Vicat Softening Point 305 °FASTM D1525
Flammability, UL94 V-0
@Thickness 1.55 mm
NA
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.585ASTM D542
Haze 0.90 - 1.0 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 87 - 89 %125 mil; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 520 - 540 °F
Middle Barrel Temperature 530 - 550 °F
Front Barrel Temperature 540 - 570 °F
Nozzle Temperature 530 - 570 °F
Melt Temperature 550 - 600 °F
Mold Temperature 170 - 200 °F
Drying Temperature 250 °F
Dry Time 3 - 12 hour
Moisture Content <= 0.020 %
Injection Pressure 1000 - 1800 psi
Back Pressure 70.0 - 150 psi
Shot Size 40 - 60 %
Screw Speed 40 - 70 rpm
 
Descriptive Properties
Holding Pressure700 to 1200 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Entec Hylex® P1010L1 HB Polycarbonate
Ravago Manufacturing Americas Hylex® P1010G10 HB Polycarbonate, 10% Fiberglass Reinforced
Ravago Manufacturing Americas Hylex® P1310G15 HB Polycarbonate, 15% Fiberglass Reinforced, UV Stabilized
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized

PENTA034 / 36044

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.