MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Feature: Injection Molding, PA66+GF50%, General Purpose

Application: Automotive (Gear Shift Housing)

CAS No. 32131-17-2 and 65997-17-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.57 g/cc1.57 g/ccASTM D792
Water Absorption 0.50 %0.50 %ASTM D570
Maximum Moisture Content 0.0900.090Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0050 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D785
Tensile Strength, Yield 230 MPa
@Thickness 3.20 mm
33400 psi
@Thickness 0.126 in
5mm/min; ASTM D638
Elongation at Break 2.0 %
@Thickness 3.20 mm
2.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Yield Strength 329 MPa
@Thickness 3.20 mm
47600 psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus 14.27 GPa
@Thickness 3.20 mm
2069 ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched 1.47 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
2.76 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
635 kV/in
@Thickness 0.0394 in
ASTM D149
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=0.750 mm
15 - 30 sec
@Thickness >=0.0295 in
 15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
 15 - 30 sec
@Thickness >=3.00 mm
15 - 30 sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FASTM D696
Melting Point 260 °C500 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
@Thickness 6.40 mm
500 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
@Thickness 6.40 mm
491 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical  120 °C
@Thickness >=0.750 mm
248 °F
@Thickness >=0.0295 in
 120 °C
@Thickness >=1.50 mm
248 °F
@Thickness >=0.0591 in
 120 °C
@Thickness >=3.00 mm
248 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  110 °C
@Thickness >=0.750 mm
230 °F
@Thickness >=0.0295 in
 110 °C
@Thickness >=1.50 mm
230 °F
@Thickness >=0.0591 in
 110 °C
@Thickness >=3.00 mm
230 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  120 °C
@Thickness >=0.750 mm
248 °F
@Thickness >=0.0295 in
 120 °C
@Thickness >=1.50 mm
248 °F
@Thickness >=0.0591 in
 120 °C
@Thickness >=3.00 mm
248 °F
@Thickness >=0.118 in
Flammability, UL94  HB
@Thickness >=0.750 mm
HB
@Thickness >=0.0295 in
 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
 HB
@Thickness >=3.00 mm
HB
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 270 °C500 - 518 °FInjection Molding
Middle Barrel Temperature 270 - 285 °C518 - 545 °FInjection Molding
Front Barrel Temperature 270 - 290 °C518 - 554 °FInjection Molding
Nozzle Temperature 270 - 290 °C518 - 554 °FInjection Molding
Melt Temperature 270 - 295 °C518 - 563 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °FInjection Molding
Drying Temperature 80.0 - 100 °C176 - 212 °FInjection Molding
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psiInjection Molding
Screw Speed 30 - 60 rpm30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose
Celanese Celstran® PA66-GF50-20 PA66, 50% Glass Reinforced
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant

PLAY146 / 148154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.