MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Feature: Injection Molding, PA66+GF50%, General Purpose

Application: Automotive (Gear Shift Housing)

CAS No. 32131-17-2 and 65997-17-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.57 g/ccASTM D792
Water Absorption 0.50 %ASTM D570
Maximum Moisture Content 0.090Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ASTM D785
Tensile Strength, Yield 2350 kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break 2.0 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Yield Strength 3350 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus 145500 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 15.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 4.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
ASTM D149
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=0.750 mm
 15 - 30 sec
@Thickness >=1.50 mm
 15 - 30 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
 >= 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 3.00 mm
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CASTM D696
Melting Point 260 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 120 °C
@Thickness >=0.750 mm
 120 °C
@Thickness >=1.50 mm
 120 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 110 °C
@Thickness >=0.750 mm
 110 °C
@Thickness >=1.50 mm
 110 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 120 °C
@Thickness >=0.750 mm
 120 °C
@Thickness >=1.50 mm
 120 °C
@Thickness >=3.00 mm
Flammability, UL94 HB
@Thickness >=0.750 mm
 HB
@Thickness >=1.50 mm
 HB
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 270 °CInjection Molding
Middle Barrel Temperature 270 - 285 °CInjection Molding
Front Barrel Temperature 270 - 290 °CInjection Molding
Nozzle Temperature 270 - 290 °CInjection Molding
Melt Temperature 270 - 295 °CInjection Molding
Mold Temperature 80.0 - 110 °CInjection Molding
Drying Temperature 80.0 - 100 °CInjection Molding
Dry Time 4.00 - 5.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPaInjection Molding
Screw Speed 30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose
Celanese Celstran® PA66-GF50-20 PA66, 50% Glass Reinforced
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant

PLAY146 / 148154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.