MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Permalyn™ 6110 Synthetic Resin
Categories: Polymer

Material Notes: Product Description: Permalyn™ 6110 Synthetic Resin, a very pale, hard, thermoplastic resin, is a pentaerythritol ester of rosin. It is produced by a special process that yields a low-odor, light-colored, very stable product. Permalyn™ 6110 Synthetic Resin is used as a resin modifier in elastomers, waxes, filmformers, and various adhesive and protective coating applications.

Application/Uses:

  • Asphalt Modification
  • Assembly
  • Automotive
  • Bookbinding
  • Building and Construction
  • Contact Adhesives
  • Footwear and Leather
  • Hot Melt Adhesives
  • Laminating
  • Packaging
  • Pressure sensitive adhesives
  • Solventborne Adhesives
  • Tapes and Labels
  • Wax Modification
Key Attributes:
  • High softening point
  • Light color
  • Low odor
  • Resistant to thermal degradation
  • Thermoplastic resin
  • Very good color stability
  • Wide solubility and compatibility range

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³
Viscosity  120 cP
@Temperature 180 °C
120 cP
@Temperature 356 °F
Melt
 440 cP
@Temperature 160 °C
440 cP
@Temperature 320 °F
Melt
 2100 cP
@Temperature 140 °C
2100 cP
@Temperature 284 °F
Melt
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 1313[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 101 °C214 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Evonik DS 50 Synthetic Resin
Eastman Permalyn™ 6110-M Synthetic Resin
Eastman Permalyn™ 5095 Synthetic Resin

PEATM5501 / 222695

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.