MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BG 30 FN05 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: PA 6, 30% glass, injection molding, halogen free flame retardant, low tendency to warp

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/in60x60x2; 260 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in60x60x2; 260 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psi5 mm/min; ISO 527-1,-2
Elongation at Break 2.4 %2.4 %5 mm/min; ISO 527-1,-2
Tensile Modulus 5.40 GPa783 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 120 MPa17400 psi2 mm/min; ISO 178-A
Flexural Modulus 5.20 GPa754 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 3.3 %3.3 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 0.00 V0.00 VSolution A; UL 746A
 550 V550 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 222 °C432 °F10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air 201 °C394 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75-1,-2
Vicat Softening Point 195 °C
@Load 5.10 kg
383 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Glow Wire Ignition Temperature  800 °C
@Thickness 1.50 mm
1470 °F
@Thickness 0.0591 in
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
IEC 60695-2-13
 900 °C
@Thickness 0.750 mm
1650 °F
@Thickness 0.0295 in
IEC 60695-2-13
 960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
Shrinkage, MD 0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.20 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD 0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.20 %
@Treatment Temp. 248 °F,
Time 4.00 hour
60x60x2; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °Finjection molding
 250 - 270 °C482 - 518 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 6.00 hour2.00 - 6.00 hour
Moisture Content 0.030 - 0.070 %0.030 - 0.070 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
Envalior Durethan® BG 30 X F30 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 30 N1 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Pocan® BF 4232 000000 PBT, 30% Glass Fiber Filled
Envalior Durethan® BG 30 X 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry

PLANW9296 / 208103

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.