Description: BRASKEM DR7052.01 Developmental Resin is a random copolymer for thin wall injection molding applications. The grade is characterized by a balanced mix of key properties e.g. good stiffness/impact balance, excellent optical properties and very high flowability. Application: - Thin wall packaging e.g. container, caps and lids
- Thin wall consumer goods e.g. Housewares, media packaging
Information provided by Braskem |