MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water resistance, low color, and consistent quality through SPC methods. Their applications include: PVC lubricants, textile softener/lubricant, floor polish, plastic additive applications, paper coating lubricant, fruit coating, agricultural sprays, car polish, and fiberglass sizing. Products are supplied as free flowing pellets; although some products may be available in powder form. Products made with these polymers will have attributes that deliver: abrasion resistance, moisture and grease resistance, surface slip and release properties, and compatibility with other polymers, pigments, and fillers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 - 0.960 g/cc0.930 - 0.960 g/cc
Viscosity 650 - 1200 cP
@Temperature 125 °C
650 - 1200 cP
@Temperature 257 °F
542-111
Brookfield Viscosity 800 cP
@Temperature 125 °C
800 cP
@Temperature 257 °F
Molecular Weight 6100 g/mol6100 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 1717
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 204 °C>= 399 °F
Ring & Ball Softening Point 106 °C223 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 2.0<= 2.0542-130
 
Descriptive Properties
Penetration Hardness 2 dmmASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® C-19 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer

PWESF9035 / 106872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.