MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It has a low softening point and low viscosity. The low softening point and low viscosity contribute to the hardness, short drying time, and excellent gloss in coatings.
    Key Attributes:
  • Low density polyethylene (PE)
  • Oxidized to provide functionality
  • Useful as a lubricant for HDPE extrusion
    Application/Uses:
  • Asphalt modification
  • Building and Construction
  • Hot Melt Adhesives
  • Pressure Sensitive Adhesives
  • Wax Modification

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 - 0.960 g/cc0.930 - 0.960 g/cc
Viscosity 1000 - 2500 cP
@Temperature 125 °C
1000 - 2500 cP
@Temperature 257 °F
V-005
Brookfield Viscosity 1500 cP
@Temperature 125 °C
1500 cP
@Temperature 257 °F
Molecular Weight 7500 g/mol7500 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 16.216.2
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 204 °C>= 399 °F
Ring & Ball Softening Point 110 °C230 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 10<= 10VCC-099
 
Descriptive Properties
Penetration Hardness <1 dmmASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® C-19 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® E-14E Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® E-14P Oxidized Low Molecular Weight Polyethylene Polymer

PWESF9034 / 106871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.