MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Ultramid® 8200 HS PA 6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over conventional lower viscosity grades. It possesses a combination of strength, stiffness and toughness properties as well as excellent heat, chemical and abrasion resistance. It is available in natural and pigmented versions.

Applications: Ultramid 8200 HS is generally recommended for application such as wiring devices, plugs, receptacles, gears, connectors, convoluted tubing, filter housings, hinges, and textile components.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.6 %1.6 %24 Hours; ISO 62
 2.7 %2.7 %50% RH; ISO 62
 9.5 %9.5 %Saturation; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psi23; ISO 527
 23.0 MPa
@Temperature 121 °C
3340 psi
@Temperature 250 °F
ISO 527
 136 MPa
@Temperature -40.0 °C
19700 psi
@Temperature -40.0 °F
ISO 527
Elongation at Break 25 %25 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Tensile Modulus 2.70 GPa392 ksiISO 527
Flexural Strength 82.0 MPa11900 psiISO 178
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 285 °C464 - 545 °F
Mold Temperature 65.0 - 80.0 °C149 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content >= 0.15 %>= 0.15 %
Injection Pressure 35.0 - 125 MPa5080 - 18100 psi
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8200 HS PA 6 (Conditioned)
Overview of materials for Nylon 6, Unreinforced
Kolon KOPA® KN136 General Purpose Nylon 6
Arkema Orgalloy® RDG 113 PA
BASF Ultramid® 8202 HS PA6 (Conditioned)

PBASG0470 / 132103

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.