MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

MRC Polymers NAXELL™ PC100H General Purpose Polycarbonate, High MFR  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:
  • High Quality, High melt PC
  • MFR can be modified between 10 to 40 g/10min
  • Can be UV Stabilized
  • Internal and external lubricant can be added
  • Can be clear to color matched

Information provided by MRC Polymers Inc.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.15 %
@Temperature 22.8 °C,
Time 86400 sec
0.15 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.17 mm
0.0050 - 0.0070 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 23 g/10 min
@Load 1.20 kg,
Temperature 300 °C
23 g/10 min
@Load 2.65 lb,
Temperature 572 °F
nominal; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.1 MPa
@Thickness 3.17 mm,
Temperature 22.8 °C
9000 psi
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D638
Elongation at Break 80 %
@Thickness 3.17 mm,
Temperature 22.8 °C
80 %
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D638
Flexural Strength 93.1 MPa
@Thickness 3.17 mm,
Temperature 22.8 °C
13500 psi
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D790
Flexural Modulus 2.28 GPa
@Thickness 3.17 mm,
Temperature 22.8 °C
330 ksi
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.5 µm/m-°C
@Temperature -40.0 - 35.0 °C
37.5 µin/in-°F
@Temperature -40.0 - 95.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
@Thickness 3.17 mm
270 °F
@Thickness 0.125 in
un-annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
@Thickness 3.17 mm
260 °F
@Thickness 0.125 in
un-annealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 78 %78 %ASTM E1348
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 260 °C480 - 500 °F
Middle Barrel Temperature 260 - 271 °C500 - 520 °F
Front Barrel Temperature 271 - 282 °C520 - 540 °F
Nozzle Temperature 271 - 282 °C520 - 540 °F
Melt Temperature 249 - 282 °C480 - 540 °F
Mold Temperature 48.9 - 93.3 °C120 - 200 °F
Drying Temperature 116 °C240 °F
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content <= 0.020 %<= 0.020 %
Dew Point <= -17.8 °C<= 0.000 °F
Drying Air Flow Rate 22.7 - 28.3 l/min0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi
Back Pressure 0.345 - 1.21 MPa50.0 - 175 psi
Cushion 0.635 cm0.250 in
Screw Speed 50 - 75 rpm50 - 75 rpm
 
Descriptive Properties
Fill RateModerate
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cyclics CBT® 100 Thermoplastic Resin
MRC Polymers NAXELL PC100H High MFR Polycarbonate
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release
Mitsubishi Iupilon® S2000UR 9.5 MFI, UV Stabilized Polycarbonate With Release

PMRC028 / 89457

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.