MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MRC Polymers NAXELL PC100H High MFR Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: NAXELL PC100H is a general purpose, high MFR Polycarbonate. This material is available in black and custom colors. It is typically used for automotive exterior applications.

Information provided by MCR Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccISO 1183
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 250 °C
20 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 61.0 MPa8850 psiISO 527
Elongation at Yield 80 %80 %ISO 527
Tensile Modulus 2.37 GPa344 ksiISO 527
Flexural Modulus 2.30 GPa334 ksiISO 178
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °Funannealed; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cyclics CBT® 100 Thermoplastic Resin
MRC Polymers NAXELL™ PC100H General Purpose Polycarbonate, High MFR
Trinseo CALIBRE™ 301 HMR FC030003 Polycarbonate Resin
MRC Polymers NAXELL™ PC110-919 General Purpose Polycarbonate, Medium High MFR
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable

PMRC5003 / 217589

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.