MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexForce™ 790 Hybrid Composite Fabric
Categories: Other Engineering Material; Composite Fibers

Material Notes: Hexcel features custom fabric design and manufacturing for optimum performance. Two or more different fibers (carbon, glass, aramid, ceramics) may be combined, different weaving solutions are possible, various produce preforms, etc.

Information provided by Hexcel

Key Words: Kevlar
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 320 microns12.6 mil
Fiber Count 2400 dtex2160 denierKevlar® 49 Fill Yarn
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 228 GPa33000 ksi3K Carbon Warp Yarn
 
Descriptive Properties
Fabric Weight (oz/yd2)6.6Dry
Nominal Construction (count/in)12.5Warp
 13Fill
Weave StylePlain

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel® HexForce™ 117 Fiber Glass Fabric
Chosun Refractories PT-165 Plastic Refractory
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
Cancarb Thermax® Powder N908 Stainless Medium Carbon Black

PHEXC663 / 101282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.