MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chosun Refractories PT-165 Plastic Refractory
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  3.85e-7 - 0.000981 GPa
@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi
@Temperature 230 °F,
Time 24.0 hour
 0.002943 - 0.005886 GPa
@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.8537 ksi
@Temperature 2460 °F,
Time 3.00 hour
 0.004905 - 0.007848 GPa
@Temperature 1500 °C,
Time 10800 sec
0.7114 - 1.138 ksi
@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength  4.90 - 9.81 MPa
@Treatment Temp. 110 °C,
Time 86400 sec
711 - 1420 psi
@Treatment Temp. 230 °F,
Time 24.0 hour
Cold Crushing Strength
 19.6 - 29.4 MPa
@Treatment Temp. 1350 °C,
Time 10800 sec
2840 - 4270 psi
@Treatment Temp. 2460 °F,
Time 3.00 hour
Cold Crushing Strength
 24.5 - 34.3 MPa
@Treatment Temp. 1500 °C,
Time 10800 sec
3560 - 4980 psi
@Treatment Temp. 2730 °F,
Time 3.00 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.97705 W/m-K
@Temperature 500 °C
6.7697 BTU-in/hr-ft²-°F
@Temperature 932 °F
 1.0585 W/m-K
@Temperature 1000 °C
7.3339 BTU-in/hr-ft²-°F
@Temperature 1830 °F
Maximum Service Temperature, Air 1650 °C3000 °Flimited
Shrinkage  -0.700 %
@Temperature 110 °C,
Time 86400 sec
-0.700 %
@Temperature 230 °F,
Time 24.0 hour
 0.20 %
@Temperature 1500 °C,
Time 10800 sec
0.20 %
@Temperature 2730 °F,
Time 3.00 hour
 0.30 %
@Temperature 1350 °C,
Time 10800 sec
0.30 %
@Temperature 2460 °F,
Time 3.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 43 %43 %
SiO2 50 %50 %
 
Descriptive Properties
Main ApplicationsHeat set Air Set Spalling resistance Volume stability Various furnace
Material Required for Estimating (kg/m3)2,400

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast AR Castable Refractory
Niobium, Nb (Columbium, Cb); Annealed Sample
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite
Momentive Performance Materials AC6041 Boron Nitride (BN) Powder
Malvern Minerals Trikup® PF Silane Treated Aluminum Hydroxide

CCHOS255 / 124199

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.