MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A387 Alloy Steel, Grade 22, Class 2  (discontinued **)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Cr-Mo alloy steel plate
High service temperature

Pressure vessel quality

Spec discontinued in 1989

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 515 - 690 MPa74700 - 100000 psi
Tensile Strength, Yield 310 MPa45000 psi
Elongation at Break 18 %18 %in 50mm
Modulus of Elasticity 200 GPa29000 ksiTypical Carbon Steel
Bulk Modulus 160 GPa23200 ksiTypical for Steel
Poissons Ratio 0.290.29Typical Carbon Steel
Shear Modulus 80.0 GPa11600 ksiTypical for Steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FTypical Carbon Steel
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FTypical Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.15 %0.15 %may vary with plate thickness
Chromium, Cr 2.0 - 2.5 %2.0 - 2.5 %
Iron, Fe 95.58 %95.58 %as balance
Manganese, Mn 0.30 - 0.60 %0.30 - 0.60 %
Molybdenum, Mo 0.90 - 1.1 %0.90 - 1.1 %
Phosphorus, P 0.035 %0.035 %
Silicon, Si 0.50 %0.50 %
Sulfur, S 0.035 %0.035 %

References for this datasheet.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A387 Alloy Steel, Grade 22, Class 1
ASTM A182, Grade F11, Class 1
ASTM A285, Grade A
ASTM A516, Grade 60
ASTM A515 Steel, grade 70

MSA38722c2 / 142882

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.