MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cumene ((CH3)2CHC6H5; iso-Propylbenzene)
Categories: Fluid; Solvent

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.8618 g/cc
@Temperature 20.0 °C
0.03113 lb/in³
@Temperature 68.0 °F
Viscosity 0.737 cP
@Temperature 25.0 °C
0.737 cP
@Temperature 77.0 °F
Molecular Weight 120.2 g/mol120.2 g/mol
Vapor Pressure 0.1000 bar
@Temperature 86.7 °C
75.00 torr
@Temperature 188 °F
Surface Tension 27.69 dynes/cm27.69 dynes/cmat 25°C; Gamma
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 32.09 bar24070 torr
Critical Temperature 357.68 °C675.82 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 60.98 J/g26.23 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 375.5 J/g161.5 BTU/lbEnthalpy of vaporization at normal boiling temperature
Thermal Conductivity 0.128 W/m-K
@Temperature 25.0 °C
0.888 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Melting Point -96.02 °C-140.8 °FAt atmospheric pressure (760 torr)
Boiling Point 38.2 °C101 °Fat 10 torr
 152.4 °C
@Pressure 0.101 MPa
306.3 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4915
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.4915
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hydrazoic Acid, HN3
Honeywell Dichloromethane
Methyl Ethyl Ketone (CH3CH2COCH3; 2-Butanone; MEK)
Molybdenum (VI) Fluoride, MoF6
Shandong Dongyue Shenzhou New Material Co Perfluoropropylenevinylether (PPVE)

VORG009 / 74520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.