MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

UBE UMERIT 1500F Metallocene LLDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical properties by being able to acquire any targeted molecular structures. Specific Notes for this Grade: UMERIT® 1500F offers various excellent properties: Superior low temperature seal property, advantageous compared to 2000F, Reduced motor load at processing, Draw resonance at high-speed drawing hardly occurs

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.913 g/cc0.0330 lb/in³ASTM D1505
Environmental Stress Crack Resistance 1000 hour1000 hourF50; ASTM D1693
Melt Flow 4.0 g/10 min4.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5151ASTM D2240
Tensile Strength, Yield 39.0 MPa5660 psiASTM D638
Elongation at Break 730 %730 %ASTM D638
Tensile Modulus 0.190 GPa27.6 ksiBending Modulus; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 99.0 °C210 °FUBE method
Vicat Softening Point 97.0 °C207 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tisan TISETILEN® Flame Retardant (V0) Polyethylene
ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
Dow Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating

PUBE001 / 71561

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.