MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Tisan TISETILEN® Flame Retardant (V0) Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include
  • Low density
  • Flexible toughness
  • Easy processability and dying
  • High performance
  • Good chemical resistance
General specifications can also include high density. TISETILEN has an excellent chemical resistance to weak acids and weak alkalis. It has good chemical resistance to strong acids, strongo alkalis, and alcohols. It has weak resistance to organic solvents, hydrocarbons, and engine fuels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Linear Mold Shrinkage 0.020 cm/cm0.020 in/in
Melt Flow 11 g/10 min11 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Izod Impact, Notched (ISO) 4.45 kJ/m²2.12 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VTS EN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 °C228 °F
Heat Distortion Temperature 78.0 - 110 °C172 - 230 °FISO 75-2
Flammability, UL94 V-0V-0
Glow Wire Test 960 °C1760 °F60695-2-10
 
Processing PropertiesMetricEnglishComments
Feed Temperature 50.0 °C122 °F
Rear Barrel Temperature 170 - 190 °C338 - 374 °FAft-1. Region Temperature
Middle Barrel Temperature 170 - 190 °C338 - 374 °FMid-2. Region Temperature
Front Barrel Temperature 170 - 190 °C338 - 374 °FPre-3. Region Temperature
Nozzle Temperature 180 °C356 °F
Drying Temperature 80.0 °C176 °FPredrying Temperature
Dry Time 1 hour1 hourPredrying Time
 
Descriptive Properties
Block Temperature40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovation Polymers Nima™ HL 18400 HDPE
Multibase Multi-Flam™ 0107 HDPE Polyethylene
Avient Maxxam™ FR PE 161-1A Polyethylene, High Density (HDPE)
Avient Maxxam® FR PE JR 165 High Density Polyethylene (HDPE)
Mitsubishi Chemical Advanced Materials TIVAR® Burnguard Flame Retardant Lining Material (ASTM Product Data Sheet)

PTIS066 / 79501

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.