MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ethanethiol (Ethyl mercaptan), C2H5SH
Categories: Fluid; Solvent

Key Words: C2H5SH
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.839 g/cc
@Temperature 20.0 °C
0.0303 lb/in³
@Temperature 68.0 °F
Viscosity 0.249 cP
@Temperature 20.0 °C
0.249 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 62.134 g/mol62.134 g/mol
Vapor Pressure 0.578948 bar
@Temperature 20.0 °C
434.248 torr
@Temperature 68.0 °F
Surface Tension 22.39 dynes/cm
@Temperature 20.0 °C
22.39 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 54.9 bar41200 torr
Critical Temperature 226 °C439 °F
Critical Density 0.300 g/cc0.0108 lb/in³
Critical Molar Volume 207 cm³/mol12.6 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 431 J/g185 BTU/lb
Specific Heat Capacity 1.187 J/g-°C
@Temperature 25.0 °C
0.2837 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Melting Point -147.9 °C-234.2 °F
Boiling Point 35.1 °C95.2 °F
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.0077
Antoine's Vapor Pressure B Parameter2497.23
Antoine's Vapor Pressure C Parameter-41.77
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)75-08-1
Chemical FormulaC2H5SH
Critical Compressibility (Zc)0.274
Dipole moment (p/C.m)5.003E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A419.6
Dynamic Viscosity Parameter B206.21
Molar Heat Capacity (298K)73.747 J/mol-K
Molar Heat Capacity of Vapor a Parameter14.9118
Molar Heat Capacity of Vapor b Parameter0.2349
Molar Heat Capacity of Vapor c Parameter-0.0001355
Molar Heat Capacity of Vapor d Parameter3.16E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Leaded Red Brass, UNS C83600, Copper Casting Alloy (Bronze SAE 40)
Methanethiol (Methyl mercaptan), CH3HS
UNS C90800, Copper Casting Alloy
LG Chemical LGflex TINTM Plasticizer

VORGS155 / 99531

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.