MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 612, Carbon Fiber Filler
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Carbon Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.06 - 1.55 g/cc0.0383 - 0.0560 lb/in³Average value: 1.26 g/cc Grade Count:29
Filler Content 8.00 - 40.0 %8.00 - 40.0 %Average value: 21.8 % Grade Count:17
Water Absorption 0.140 - 1.27 %0.140 - 1.27 %Average value: 0.269 % Grade Count:14
Additive Loading 20.0 - 30.0 %20.0 - 30.0 %Average value: 27.5 % Grade Count:4
Linear Mold Shrinkage 0.000500 - 0.00900 cm/cm0.000500 - 0.00900 in/inAverage value: 0.00254 cm/cm Grade Count:25
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106 - 120106 - 120Average value: 117 Grade Count:7
Tensile Strength, Ultimate 40.0 - 231 MPa5800 - 33500 psiAverage value: 145 MPa Grade Count:30
Tensile Strength, Yield 50.0 - 200 MPa7250 - 29000 psiAverage value: 127 MPa Grade Count:3
Elongation at Break 1.00 - 70.0 %1.00 - 70.0 %Average value: 6.53 % Grade Count:31
Modulus of Elasticity 1.52 - 27.6 GPa220 - 4000 ksiAverage value: 13.0 GPa Grade Count:27
Flexural Yield Strength 101 - 348 MPa14600 - 50500 psiAverage value: 253 MPa Grade Count:27
Flexural Modulus 3.34 - 22.4 GPa484 - 3250 ksiAverage value: 13.0 GPa Grade Count:27
Izod Impact, Notched 0.427 - 1.28 J/cm0.800 - 2.40 ft-lb/inAverage value: 0.886 J/cm Grade Count:25
Izod Impact, Unnotched 2.40 - 10.7 J/cm4.50 - 20.0 ft-lb/inAverage value: 6.64 J/cm Grade Count:22
Izod Impact, Notched (ISO) 20.0 - 20.0 kJ/m²
@Temperature -30.0 - -30.0 °C
9.52 - 9.52 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 20.0 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 94.0 - 94.0 kJ/m²
@Temperature -30.0 - -30.0 °C
44.7 - 44.7 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 94.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 5.50 J/cm² - NB26.2 ft-lb/in² - NBAverage value: 8.17 J/cm² Grade Count:4
 5.10 J/cm² - NB
@Temperature -40.0 - 0.000 °C
24.3 ft-lb/in² - NB
@Temperature -40.0 - 32.0 °F
Average value: 5.20 J/cm² Grade Count:2
Charpy Impact, Notched 0.920 - 5.60 J/cm²4.38 - 26.7 ft-lb/in²Average value: 2.07 J/cm² Grade Count:4
 0.700 - 2.00 J/cm²
@Temperature -40.0 - 0.000 °C
3.33 - 9.52 ft-lb/in²
@Temperature -40.0 - 32.0 °F
Average value: 1.35 J/cm² Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.100 - 1.00e+6 ohm-cm0.100 - 1.00e+6 ohm-cmAverage value: 32100 ohm-cm Grade Count:20
Surface Resistance 100 - 1.00e+10 ohm100 - 1.00e+10 ohmAverage value: 170000 ohm Grade Count:10
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 - 218 °C329 - 424 °FAverage value: 196 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 131 - 221 °C268 - 430 °FAverage value: 203 °C Grade Count:15
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 227 °C140 - 440 °FAverage value: 201 °C Grade Count:27
Flammability, UL94 HB - V-0HB - V-0Grade Count:21
 
Processing PropertiesMetricEnglishComments
Processing Temperature 252 - 279 °C485 - 535 °FAverage value: 266 °C Grade Count:10
Melt Temperature 249 - 300 °C480 - 572 °FAverage value: 271 °C Grade Count:15
Mold Temperature 60.0 - 250 °C140 - 482 °FAverage value: 85.6 °C Grade Count:24
Drying Temperature 79.4 - 100 °C175 - 212 °FAverage value: 80.3 °C Grade Count:13
Moisture Content 0.0150 - 0.200 %0.0150 - 0.200 %Average value: 0.182 % Grade Count:13
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:11
Injection Pressure 68.9 - 124 MPa10000 - 18000 psiAverage value: 96.5 MPa Grade Count:21

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Carbon Fiber Filled
Overview of materials for Nylon 610, Glass Reinforced
Overview of materials for Nylon 6, 50% Glass Fiber Filled
Overview of materials for Nylon 6, Glass/Mineral Reinforced
Overview of materials for Nylon 610, Carbon Fiber Filled

O2604 / 78049

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.