MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Bormed™ LE6609-PH LDPE for Pharmaceutical Blow Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Bormed LE6609-PH is a LD-polyethylene produced in a high-pressure process intended for blow molding of soft and flexible packages for pharmaceutical products.

Bormed LE6609-PH can be used in "blow-fill and seal" machines for the production of ampoules and bottles. The product can also be used for pharmaceutical products manufactured with other conversion techniques such as injection molding and film blowing. LE6609-PH will withstand heating up to 110°C and therefore units made from this product may be steam treated to max 110°C.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353ISO 868
Tensile Strength, Yield 14.0 MPa2030 psi50 mm/min; ISO 527-2
Tensile Modulus 0.400 GPa58.0 ksiAt 1 mm/min; ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °C129 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 165 - 200 °C329 - 392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene
Borealis Bormed™ LE6601-PH LDPE for Pharmaceutical Blow Molding
Borealis BS2581 High Density Polyethylene for Blow Molding
Huntsman PE7076 Profile Extrusion Polyethylene
Borealis Bormed™ LE6607-PH LDPE for Pharmaceutical Blow Molding

PBOREA079 / 27386

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.