MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BS2581 High Density Polyethylene for Blow Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, household and chemical containers such as detergents, cleaners, motor oils, and other bottles and containers up to 10 liters.

Information provided by Borealis AG

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.958 g/cc0.0346 lb/in³ISO 1183
Environmental Stress Crack Resistance 100 hour100 hourAntarox 10%, F50; ASTM D1693-A
Melt Flow  0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 1.3 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.3 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 28 g/10 min
@Load 21.6 kg,
Temperature 190 °C
28 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Tensile Strength, Yield 29.0 MPa4210 psi50mm/min; ISO 527-2
Elongation at Yield 8.0 %8.0 %50mm/min; ISO 527-2
Tensile Modulus 1.30 GPa189 ksi1mm/min; ISO 527-2
Flexural Modulus 1.40 GPa203 ksi1mm/min; ISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 170 - 190 °C338 - 374 °F
Die Temperature 175 - 190 °C347 - 374 °F
Melt Temperature 170 - 200 °C338 - 392 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BB2581 HDPE for Blow Molding
Braskem HB 0155 HDPE Blow Molding Polyethylene
Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Borealis BS4641 High Density Polyethylene

PBOREA336 / 108596

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.