MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M 2497ST High-Temperature Tear Resistant Polyester Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ High-Temperature Tear Resistant Polyester Tape 2497ST is designed for use in masking applications where sliver resistance and clean removal are required.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 83.8 microns3.30 milASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 113.75 MPa16498 psiASTM D3756
Elongation at Break 112 %112 %ASTM D3756
Peel Strength 0.18626 kN/m1.0625 plito Steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °Fup to 30 mins
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Adhesive TypeRubber/resin
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 8992L Polyester Tape
3M 8911 Polyester Tape
3M 8421 Polyester Tape
3M 8401 Polyester Tape

PMM33978 / 168725

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.