MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt DISTITRON® 120 V2,5 Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, DCPD

Appearance: Yellow - Light - Transparent

Main resin characteristics: Clear, unaccelerated

Main applications: Profiles

Molding information: Pultrusion

Curing cycle: 24h at 23°C + 2h at 100°C + 1h at 100°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Solids Content 60 - 64 %60 - 64 %MT-CU001C
Brookfield Viscosity 180 - 270 cP180 - 270 cPsp 2 rpm 20; MT-CUT25V
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4242ASTM D 2583
Tensile Strength 60.0 MPa8700 psiISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Tensile Modulus 3.20 GPa464 ksiISO 527
Flexural Strength 110 MPa16000 psiISO 178/B
Flexural Modulus 3.10 GPa450 ksiISO 178/B
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75 -2A
Glass Transition Temp, Tg 120 °C248 °FASTM E 1545
 
Processing PropertiesMetricEnglishComments
Cure Time  6.00 - 7.50 min
@Temperature 82.2 °C
0.100 - 0.125 hour
@Temperature 180 °F
SPI; Reactivity at 82,2°C + 2% PBO50; RS.03.G
 7.00 - 9.50 min
@Temperature 82.2 °C
0.117 - 0.158 hour
@Temperature 180 °F
LPE; Reactivity at 82,2°C + 2% PBO50; RS.03.G
Shelf Life 6.00 Month6.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm205-235°CRS.08.G; Reactivity, at 82,2°C + 2% PBO50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. EXTER S® S 402 Isophthalic Resin
Polynt DISTITRON® 135 SX Unsaturated Polyester Resin
Avient Maxxam™ PPR-20G Nat Polypropylene Homopolymer (PP Homopolymer)
Asahi Kasei DELPET™ 720V Acrylic (PMMA), Standard Grade
Polynt DISTITRON® 100 SW Unsaturated Polyester Resin

PPOLYN9284 / 231879

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.