MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Maxxam™ PPR-20G Nat Polypropylene Homopolymer (PP Homopolymer)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Filler Content 20 %20 %Unspecified
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inASTM D955
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 64.1 MPa9300 psiType I, 51 mm/min; ASTM D638
Elongation at Break 10 %10 %Type I, 51 mm/min; ASTM D638
Flexural Strength 90.3 MPa13100 psiASTM D790
Flexural Modulus 3.52 GPa511 ksiASTM D790
Izod Impact, Notched 0.690 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.29 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Unnotched 3.10 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
5.81 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
@Thickness 3.18 mm
315 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Mold Temperature 16.0 - 50.0 °C60.8 - 122 °F
 
Descriptive Properties
AppearanceNatural Color
FeaturesChemically Coupled
 General Purpose
 Homopolymer
Filler / ReinforcementGlass Fiber Reinforcement
FormsPellets
Generic MaterialPP Homopolymer
Generic NamePolypropylene Homopolymer (PP Homopolymer)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 30 S1 NAT. (1383) PA, Cold-Impact Resistant, 30% Glass Filled, Natural
Avient Maxxam™ NT-818.G002-1000 Polypropylene
Avient Maxxam™ NT-818.B001-8000 Polypropylene
Avient Maxxam™ MN-818.S001-8000 Polypropylene
Avient Maxxam™ DC-818.G001-8000 Polypropylene

PH0POL0662 / 145231

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.