MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® PSB 286 PA6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.

Available in: North America

Product Applications: This grade has high fluidity and good mould release. It is particularly suitable for the production of technical moldings with fast injection cycles.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183/A
Water Absorption 1.3 %
@Temperature 23.0 °C,
Time 86400 sec
1.3 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/in
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527 Type 1A
Tensile Strength, Yield 85.0 MPa12300 psiISO 527 type 1 A
Elongation at Break 65 %65 %ISO 527 Type 1A
Tensile Modulus 3.00 GPa435 ksiISO 527 Type 1A
Flexural Strength 115 MPa16700 psiISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.43.4IEC 60250
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75/Af
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
1210
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
1210
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
1210
Glow Wire Flammability Index  700 °C
@Thickness 0.800 mm
1290 °F
@Thickness 0.0315 in
ISO 60695-2-12
 700 °C
@Thickness 1.60 mm
1290 °F
@Thickness 0.0630 in
ISO 60695-2-12
 750 °C
@Thickness 3.20 mm
1380 °F
@Thickness 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 230 - 235 °C446 - 455 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone235-240°C
Mixing Zone235-245°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 7335F NC010 PA6
Celanese Rynite® 408 NC010 PET
Envalior Durethan® B 30 S FN30 000000 Nylon 6 (PA6), Dry
Celanese Rynite® 530 BK503 PET-GF30
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized

PRHOD802 / 138033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.