MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® PSB 286 PA6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.

Available in: North America

Product Applications: This grade has high fluidity and good mould release. It is particularly suitable for the production of technical moldings with fast injection cycles.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183/A
Water Absorption 1.3 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm
Linear Mold Shrinkage, Transverse 0.016 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527 Type 1A
Tensile Strength, Yield 85.0 MPaISO 527 type 1 A
Elongation at Break 65 %ISO 527 Type 1A
Tensile Modulus 3000 MPaISO 527 Type 1A
Flexural Strength 115 MPaISO 178
Flexural Modulus 2800 MPaISO 178
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 5.50 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.4IEC 60250
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 222 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75/Af
Flammability, UL94 V-2
@Thickness 0.800 mm
1210
 V-2
@Thickness 1.60 mm
1210
 V-2
@Thickness 3.20 mm
1210
Glow Wire Flammability Index 700 °C
@Thickness 0.800 mm
ISO 60695-2-12
 700 °C
@Thickness 1.60 mm
ISO 60695-2-12
 750 °C
@Thickness 3.20 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 230 - 235 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone235-240°C
Mixing Zone235-245°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 7335F NC010 PA6
Celanese Rynite® 408 NC010 PET
Envalior Durethan® B 30 S FN30 000000 Nylon 6 (PA6), Dry
Celanese Rynite® 530 BK503 PET-GF30
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized

PRHOD802 / 138033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.