MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems VisiJet M100 3-D Printer Model Material
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic

Material Notes: The InVision SR (standard resolution) 3-D printer delivers key advantages compared to other 3-D modeling technologies — superior model quality, durable photopolymer materials, surface finish and feature detail, and the ability to build complex models or patterns. Choose from five model material colors - black, blue, red, grey, and white. Reported here is preliminary tech data for the cured plastic models.

Information provided by 3D Systems Corporation.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccCured
Ash 0.010 %0.010 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.0 MPa3480 psiASTM D638
Elongation at Break 15.6 %15.6 %ASTM D638
Tensile Modulus 0.7750 GPa112.4 ksiASTM D638
Flexural Strength 42.1 MPa6100 psiASTM D790
Flexural Modulus 0.110 GPa16.0 ksiASTM D790
Izod Impact, Notched 0.133 J/cm0.250 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS Lustran® 308 ABS, Medical Grade
3D Systems VisiJet® M3 Techplast
3D Systems Accura® 40 Plastic for SLA® Systems
Stratasys® PC Polycarbonate for 3D Printing
Stratasys® Ultem 9085 for Rapid Prototyping

PTHREED0 / 70244

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.