The InVision SR (standard resolution) 3-D printer delivers key advantages compared to other 3-D modeling technologies — superior model quality, durable photopolymer materials, surface finish and feature detail, and the ability to build complex models or patterns. Choose from five model material colors - black, blue, red, grey, and white. Reported here is preliminary tech data for the cured plastic models. Information provided by 3D Systems Corporation. |
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |