MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³ISO 1183
Moisture Absorption 1.10 %
@Temperature 23.0 °C
1.10 %
@Temperature 73.4 °F
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inEurotec
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inEurotec
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Tensile Modulus 9.00 GPa1310 ksiISO 527
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
 35.0 kJ/m²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °F[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FISO 75
Vicat Softening Point 205 °C
@Load 5.10 kg
401 °F
@Load 11.2 lb
ISO 306
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Ignition Temperature 850 °C
@Thickness 2.00 mm
1560 °F
@Thickness 0.0787 in
IEC 60695
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 250 °C446 - 482 °F
Feed Temperature 60.0 - 80.0 °C140 - 176 °FThroat
Mold Temperature 40.0 - 90.0 °C104 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.20 %<= 0.20 %ISO 960
Hold Pressure 50.0 - 100 MPa7250 - 14500 psi
 
Descriptive Properties
Back PressureLow
Injection SpeedMedium - Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurotec® Tecomid® NB30 BK EF PA6, unfilled, black, suitable for electrostatic powder coating
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural
Epsan Eplamid 6 FX0 NC Q1B501 Polyamide 6, Halogen Free
Envalior Durethan® B 30 S FN30 000000 Nylon 6 (PA6), Dry
Envalior Durethan® B 30 S F30 000000 Nylon 6 (PA6), Dry

PEUROS073 / 147063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.