MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epsan Eplamid 6 FX0 NC Q1B501 Polyamide 6, Halogen Free
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Flame retardant for injection molding. Halogen and phosphorus free flame retardant grade, compliance with RoHs derivatives, with rating UL94 V0 and glow-wire at 960°C, which is used in many sectors of industry.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inParallel; ISO 294-4
 0.014 cm/cm0.014 in/inNormal; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 75.0 MPa10900 psiISO 527-2
Elongation at Break 4.0 %4.0 %ISO 527-2
Tensile Modulus 3.70 GPa537 ksiISO 527-2
Flexural Strength 110 MPa16000 psiISO 178
Flexural Modulus 3.40 GPa493 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VEN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75-2/A
Vicat Softening Point 195 °C383 °FISO 306/B50
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
EN 60695-11-10
Glow Wire Ignition Temperature 750 °C
@Thickness 0.800 mm
1380 °F
@Thickness 0.0315 in
EN 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epsan Eplamid 6 NC HV A3,6 Polyamide 6
Epsan Eplamid 66 GFI 20 NC Q1C0A801 Polyamide 66
Epsan Eplamid 6 CBR 30 NC Q1D001 Polyamide 6
Epsan Eplamid 6 CBR 30 BK Q1D001 Polyamide 6
Epsan Eplamid 6 CBR 15 NC Q1B501 Polyamide 6

PEPSAN024 / 186338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.