MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayfol® CR 6-2 000000 Polycarbonate + PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Characterization: Bayfol CR 6-2 000000 is an extrusion film based on Makrolon® (PC)/ Polyester (PBT) blend.

Properties / Applications: Bayfol CR 6-2 000000 has advantages over standard polycarbonate films in terms of dynamic strength, dimensional stability and cold formability. This film, which is virtually galre-free and has excellent scratch resistance, has been developed especially for critical graphic applications and comprises a unique surface combination. Typical applications are automotive, keypads, membrane switches, hand held electronics, appliance, nameplates, touch panels and FIM - film insert molding decoration. Bayfol CR 6-2 000000 is available in various standard thicknesses from 0.005 ” to 0.012 ” (125 microns to 300 microns). Other thicknesses are available on request. The surface combination of Bayfol CR 6-2 000000 is one side fine velvet and one side very fine matte for printability. As with any product, use of Bayfol CR 6-2 000000 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
Water Absorption 0.35 %
@Time 86400 sec
0.35 %
@Time 24.0 hour
immersion; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.8 MPa8090 psiASTM D882
Tensile Strength, Yield 59.6 MPa8650 psiASTM D882
Elongation at Break 125 %125 %ASTM D882
Tear Strength 168 kN/m960 pliInitiation; ASTM D1004
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 20.0 - 120 °C
44.4 µin/in-°F
@Temperature 68.0 - 248 °F
DIN 53752
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 20.0 - 120 °C
44.4 µin/in-°F
@Temperature 68.0 - 248 °F
DIN 53752
Shrinkage  <= 0.20 %
@Temperature 90.0 °C,
Time 3600 sec
<= 0.20 %
@Temperature 194 °F,
Time 1.00 hour
transverse; IEC 60674-2
 <= 0.40 %
@Temperature 90.0 °C,
Time 3600 sec
<= 0.40 %
@Temperature 194 °F,
Time 1.00 hour
parallel; IEC 60674-2
 
Optical PropertiesMetricEnglishComments
Gloss 3.0 - 10 %3.0 - 10 %60° top side, black inked second surface; ASTM D2457
Yellow Index 1.0 %1.0 %ASTM E313
Transmission, Visible >= 80 %>= 80 %ASTM D1003
 
Descriptive Properties
AvailabilityEurope
 Near East/Africa
 North America
 South and Central America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayfol® CR 1-4 000000 Polycarbonate + PBT
Covestro Makrolon® 6267 Polycarbonate, Flame Retardant Grade
Covestro Bayfol® AS-A 2-4 Polycarbonate + PBT
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade

PB09749 / 92589

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.