MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  50.0 MPa
@Temperature 120 °C
7250 psi
@Temperature 248 °F
 60.0 MPa
@Temperature 90.0 °C
8700 psi
@Temperature 194 °F
 75.0 MPa
@Temperature 60.0 °C
10900 psi
@Temperature 140 °F
 90.0 MPa
@Temperature 23.0 °C
13100 psi
@Temperature 73.4 °F
Elongation at Break  1.6 %
@Temperature 120 °C
1.6 %
@Temperature 248 °F
 1.9 %
@Temperature 90.0 °C
1.9 %
@Temperature 194 °F
 2.2 %
@Temperature 60.0 °C
2.2 %
@Temperature 140 °F
 2.5 %
@Temperature 23.0 °C
2.5 %
@Temperature 73.4 °F
Tensile Modulus  3.80 GPa
@Temperature 120 °C
551 ksi
@Temperature 248 °F
 4.30 GPa
@Temperature 90.0 °C
624 ksi
@Temperature 194 °F
 4.70 GPa
@Temperature 60.0 °C
682 ksi
@Temperature 140 °F
 5.10 GPa
@Temperature 23.0 °C
740 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched  3.00 J/cm²
@Temperature -20.0 °C
14.3 ft-lb/in²
@Temperature -4.00 °F
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.550 J/cm²
@Temperature -20.0 °C
2.62 ft-lb/in²
@Temperature -4.00 °F
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °F
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °F
Vicat Softening Point 145 °C
@Load 5.00 kg
293 °F
@Load 11.0 lb
Flammability, UL94 V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
Oxygen Index 31 %31 %
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 100 - 120 °C212 - 248 °F
Drying Temperature 120 - 130 °C
@Time 10800 sec
248 - 266 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized

PLATH9843 / 177539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.