MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mateck Fused Silica IR Grade (SiO2)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.21 g/cc
@Temperature 20.0 °C
0.0798 lb/in³
@Temperature 68.0 °F
Solubility 0.00 ppm0.00 ppm
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 73.6 GPa10700 ksi
Poissons Ratio 0.170.17
Shear Modulus 31.4 GPa4550 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.00 µm/m-°C
@Temperature -50.0 - 50.0 °C
2.22 µin/in-°F
@Temperature -58.0 - 122 °F
Specific Heat Capacity 0.728 J/g-°C0.174 BTU/lb-°F
Thermal Conductivity 1.35 W/m-K9.37 BTU-in/hr-ft²-°F
Melting Point 1900 °C3450 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.4131
@Wavelength 3243.9 nm
1.4131
@Wavelength 3243.9 nm
 1.4494
@Wavelength 1083 nm
1.4494
@Wavelength 1083 nm
 1.4584
@Wavelength 587.6 nm
1.4584
@Wavelength 587.6 nm
nd
 1.4601
@Wavelength 546.1 nm
1.4601
@Wavelength 546.1 nm
at ne
 1.4696
@Wavelength 404.6 nm
1.4696
@Wavelength 404.6 nm
 1.615
@Wavelength 170 nm
1.615
@Wavelength 170 nm
IR Transmittance  87 %
@Wavelength 3000 nm
87 %
@Wavelength 3000 nm
Internal Transmittance
 95.5 %
@Wavelength 2800 nm
95.5 %
@Wavelength 2800 nm
Internal Transmittance
UV Transmittance  22 %
@Wavelength 220 nm
22 %
@Wavelength 220 nm
Internal Transmittance
 52.5 %
@Wavelength 240 nm
52.5 %
@Wavelength 240 nm
Internal Transmittance
 99.9 %
@Wavelength 280 nm
99.9 %
@Wavelength 280 nm
Internal Transmittance
 
Descriptive Properties
Thermal Coefficient of Refractive Index1E-05at nc microns for +20 °C
Transmission Range (microns)0.18 - 3.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mateck Fused Silica UV-VIS Grade (SiO2)
Ceradyne Thermo-Sil® HS Fused Silica
Ceradyne Thermo-Sil® UHS Fused Silica
Fused Quartz
Mateck Sapphire (Al2O3)

CMAT046 / 87730

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.