MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mateck Fused Silica IR Grade (SiO2)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.21 g/cc
@Temperature 20.0 °C
Solubility 0.00 ppm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 73.6 GPa
Poissons Ratio 0.17
Shear Modulus 31.4 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.00 µm/m-°C
@Temperature -50.0 - 50.0 °C
Specific Heat Capacity 0.728 J/g-°C
Thermal Conductivity 1.35 W/m-K
Melting Point 1900 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4131
@Wavelength 3243.9 nm
 1.4494
@Wavelength 1083 nm
 1.4584
@Wavelength 587.6 nm
nd
 1.4601
@Wavelength 546.1 nm
at ne
 1.4696
@Wavelength 404.6 nm
 1.615
@Wavelength 170 nm
IR Transmittance 87 %
@Wavelength 3000 nm
Internal Transmittance
 95.5 %
@Wavelength 2800 nm
Internal Transmittance
UV Transmittance 22 %
@Wavelength 220 nm
Internal Transmittance
 52.5 %
@Wavelength 240 nm
Internal Transmittance
 99.9 %
@Wavelength 280 nm
Internal Transmittance
 
Descriptive Properties
Thermal Coefficient of Refractive Index1E-05at nc microns for +20 °C
Transmission Range (microns)0.18 - 3.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mateck Fused Silica UV-VIS Grade (SiO2)
Ceradyne Thermo-Sil® HS Fused Silica
Ceradyne Thermo-Sil® UHS Fused Silica
Fused Quartz
Mateck Sapphire (Al2O3)

CMAT046 / 87730

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.