MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay LTF 318B Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: LTM317-1B is an epoxy resin matrix specifically developed for the production of 150°C (302°F) capable mold tooling using vacuum bag processing. LTM317-1B, which can be supplied in both standard prepreg and ZPREG selectively impregnated formats, offers 65°C (149°F) initial cure capability, long out life and, after post-cure, resistance to thermal cycling up to 150°C (302°F). LTM317-1B can be used in combination with LTF318B ZPREG selective impregnation technology surface films and with LTS317 syntactic plies to achieve a high quality surface finish by vacuum-bag processing, thereby creating many new practical possibilities’ for the manufacture of affordable, high quality, composite tooling.

Features & Benefits:

  • 21 days out life at 21°C (70°F) for LTM317-1B and ZPREG format
  • 7 days out life at 21°C (70°F) for LTF3818
  • 12 months storage at -18°C (0°F)
  • 65°C (149°F) initial cure
  • DMA E’ onset Tg of 170°C (338°F) after post-cure
  • 150°C (302°F) continuous service temperature
  • Compatible syntactic ply LTS317 (PDS1181) for improved surface quality
  • Can also be supplied for autoclave processing

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³Cured resin
Viscosity  1.1 cP
@Temperature 100 °C
1.1 cP
@Temperature 212 °F
Dynamic, 2°/min
 2.0 cP
@Temperature 80.0 °C
2.0 cP
@Temperature 176 °F
Dynamic, 2°/min
 11 cP
@Temperature 110 °C
11 cP
@Temperature 230 °F
Dynamic, 2°/min
 11 cP
@Temperature 60.0 °C
11 cP
@Temperature 140 °F
Dynamic, 2°/min
 110 cP
@Temperature 40.0 °C
110 cP
@Temperature 104 °F
Dynamic, 2°/min
Storage Temperature -18.0 °C-0.400 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.30 - 4.80 µm/m-°C
@Temperature 30.0 - 180 °C
2.39 - 2.67 µin/in-°F
@Temperature 86.0 - 356 °F
Carbon
 11.9 - 13.5 µm/m-°C
@Temperature 30.0 - 180 °C
6.61 - 7.50 µin/in-°F
@Temperature 86.0 - 356 °F
Glass
Maximum Service Temperature, Air 150 °C302 °F
Glass Transition Temp, Tg 90.0 °C194 °FDMA E' onset Tg, 5 hrs at 80°C
 110 °C230 °FDMA E' onset Tg, 2 hrs at 100°C, 30 min dwell at 80°C
 
Processing PropertiesMetricEnglishComments
Cure Time 300 min
@Temperature 80.0 °C
5.00 hour
@Temperature 176 °F
Gel Time 8.00 min8.00 min2 hrs at 100°C with dwell at 80°C
 60.0 min
@Temperature 80.0 °C
60.0 min
@Temperature 176 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Hexcel® HexPly® F593 Epoxy Resin
Solvay CYCOM® 7668 Epoxy Resin
Solvay CYCOM® 7714 Epoxy Resin

PCYTED199 / 180501

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.