MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2111 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, non-sag, non-drip and improved impact strength properties are required. This easy-to-use two part adhesive system contains no volatile solvents, readily cures at room temperature, and bonds to most materials including glass and glass fabrics, ceramics, wood, leather, most metals, and many plastics. Fully cured TRA-BOND 2111 is strong, tough, resilient, has superior mechanical impact and thermal shock resistance characteristics, and is also highly resistant to weather, water, gases and vapors, most petroleum products and fuels, salts, mild acids and alkalis, and many other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccMixed
Volatile Organic Compounds (VOC) Content 31.2 g/l31.2 g/l
Water Absorption 3.3 %3.3 %After 24 hours
Viscosity 40000 cP
@Temperature 25.0 °C
40000 cP
@Temperature 77.0 °F
Mixed (T-F spindle, 10 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282
Elongation at Yield 26 %26 %
Adhesive Bond Strength 24.1 MPa3500 psiLap shear, alum to alum
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.50e+8 ohm-cm9.50e+8 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C
@Temperature 20.0 °C
30.6 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Glass Transition Temp, Tg 45.0 °C113 °FUltimate Tg
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.531.53
 
Processing PropertiesMetricEnglishComments
Cure Time 480 min8.00 hour4 hrs @ 25°C + 4 hrs @ 65°C-plus
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 20 min20 min100 grams
 40 min40 min25 grams
 
Descriptive Properties
Color Hazy White
Mix Ratio, parts by weight100/30Resin/Hardener
Working Life hours 125 grams
Working Life minutes 20100 grams

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
Aptek 2120 PMF Low modulus urethane staking compound
Aptek 2100-A7C/B Low modulus urethane staking compound
Tra-Con Tra-Bond 2116 Low Vapor Pressure Epoxy Staking Compound
Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound

PTRAC012 / 70940

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.