MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilon® BGM-65 X V0 PA6-(GF+MD)65
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties:
  • Halogen and phosphorous-free
  • Low smoke density
  • UL94 V-0 at 1.5 mm wall thickness
  • Exceptional high oxygen index
  • High stiffness
Grilon BGM-65 X V0 is typically used for electrical applications such as switches, plugs, lamp parts, coil former bobbins, and protective housings.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³Dry; ISO 1183
Water Absorption 5.0 %5.0 %Sim. to ISO 62
Moisture Absorption 1.50 %1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psiConditioned; ISO 527-1/-2
 120 MPa17400 psiDry; ISO 527-1/-2
Elongation at Break 1.0 %1.0 %Dry; ISO 527-1/-2
 3.0 %3.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 7.10 GPa1030 ksiConditioned; ISO 527-1/-2
 11.5 GPa1670 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cm1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dry; IEC 60250
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Conditioned; IEC 60250
Dielectric Strength 29.0 kV/mm737 kV/inConditioned; IEC 60243-1
 33.0 kV/mm838 kV/inDry; IEC 60243-1
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
Dry; IEC 60250
 0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
Conditioned; IEC 60250
Comparative Tracking Index 500 V500 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-1/-2
Melting Point 222 °C432 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C176 - 230 °FLong Term; ISO 2578
 160 °C320 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-1/-2
Flammability, UL94 V-0V-0IEC 60695-11-10
 V-0
@Temperature 1.50 °C
V-0
@Temperature 34.7 °F
IEC 60695-11-10
Oxygen Index 65 %65 %ISO 4589-1/-2
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
 Lighting
FormGranules
ProcessingInjection Molding
Special CharacteristicsFlame retardant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
Wellman Wellamid® MRGF30/10 42H-NBK1 Nylon 6, 30% Mineral and 10% Glass Reinforced
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12
EMS-Grivory Grilamid® L 16 W 20 black 9995 PA12

PGRH191 / 156900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.