MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication Systems through the world.

Comments: low viscosity

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ASTM D792
Melt Flow 70 g/10 min
@Load 2.16 kg,
Temperature 235 °C
70 g/10 min
@Load 4.76 lb,
Temperature 455 °F
ASTM D1238R
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373ASTM D2240
Tensile Strength at Break >= 54.0 MPa>= 7830 psiASTM D638
Tensile Strength, Yield 42.0 MPa6090 psiASTM D638
Elongation at Break >= 250 %>= 250 %ASTM D638
Flexural Strength 55.0 MPa7980 psiASTM D790
Flexural Modulus 1.42 GPa206 ksiASTM D790
Izod Impact, Notched 0.490 J/cm0.918 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 °C446 °FFlange Temperature for T-Die Cast Film Extrusion
Feed Temperature 40.0 °C104 °FInjection Molding
Zone 1 190 °C374 °FFor T-Die Cast Film Extrusion
 190 °C374 °FInjection Molding
 230 °C446 °FFor 8x1 mm Tube Extrusion
Zone 2 200 °C392 °FInjection Molding
 210 °C410 °FFor T-Die Cast Film Extrusion
 225 °C437 °FFor 8x1 mm Tube Extrusion
Zone 3 210 °C410 °FInjection Molding
 220 °C428 °FFor 8x1 mm Tube Extrusion
 230 °C446 °FFor T-Die Cast Film Extrusion
Zone 4 210 °C410 °FInjection Molding
 215 °C419 °FFor 8x1 mm Tube Extrusion
Zone 5 200 °C392 °FInjection Molding
Die Temperature 230 °C446 °FFor T-Die Cast Film Extrusion
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection Molding
Injection Velocity 100 mm/sec3.94 in/secInjection Molding
Die Opening 0.0400 cm0.0157 inFor T-Die Cast Film Extrusion
Roll Temperature 50.0 °C122 °FChill Roll Temperature for T-Die Cast Film Extrusion
Drying Temperature 80.0 °C176 °FOption 1
 100 °C212 °FOption 2
 110 °C230 °FOption 3
Dry Time 2 - 4 hour2 - 4 hourOption 3
 4 - 6 hour4 - 6 hourOption 2
 6 - 8 hour6 - 8 hourOption 1
Injection Pressure 40.0 - 50.0 MPa5800 - 7250 psiInjection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
Hold Pressure 25.0 - 50.0 MPa3630 - 7250 psiInjection Molding
Back Pressure 5.00 MPa725 psiInjection Molding
Screw Speed 15 - 76 rpm15 - 76 rpmFor 8x1 mm Tube Extrusion
 
Descriptive Properties
C/R3-3.5:1For 8x1 mm Tube Extrusion
Calibrating Vacuum100 mbarFor 8x1 mm Tube Extrusion
Calibration 9.95 mmFor 8x1 mm Tube Extrusion
Compression Ratio2.5-3.5:1Injection Molding
 min 3:1For 8x1 mm Tube Extrusion
Die Diameter16 mmFor 8x1 mm Tube Extrusion
Die Width300 mmFor T-Die Cast Film Extrusion
Extruder Barmag, Screw Diameter = 30 mmFor T-Die Cast Film Extrusion
Extruder Characteristics65 mm screw diameterFor 8x1 mm Tube Extrusion
Film Thickness60 micronsFor T-Die Cast Film Extrusion
Flight Depth in the Feeding Zone10-15% of Screw DiameterInjection Molding
Flight Depth in the Metering Zone5-7% of Screw DiameterInjection Molding
Haul Off Speed5 m/minFor T-Die Cast Film Extrusion
Haul Speed10-55 m/minFor 8x1 mm Tube Extrusion
L/D Ratio25:1For 8x1 mm Tube Extrusion
 min 20:1Injection Molding
Length of Compression Zone25-45% of total screw lengthInjection Molding
 30% of screw lengthFor 8x1 mm Tube Extrusion
Length of Feeding Zone20-40% of total screw lengthInjection Molding
 30-40% of screw lengthFor 8x1 mm Tube Extrusion
Length of Metering Zone30-45% of screw lengthFor 8x1 mm Tube Extrusion
 35-45% of total screw lengthInjection Molding
Mandrel Diameter12 mmFor 8x1 mm Tube Extrusion
Peripheral Screw Speed10 m/minInjection Molding
Water Temperature10-18°CFor 8x1 mm Tube Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ashley Polymers Ashlene® TD930H Nylon 12
Evonik VESTOSINT® 1101 white Polyamide 12
Evonik VESTOSINT® 1111 colored Polyamide 12
Evonik VESTOSINT® 2070 natural color Polyamide 12
Akro-Plastic Akromid® A3 1 natural PA 6.6 Dry

PUBE104 / 71664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.