Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness. Key features and benefits are: - Excellent stiffness to weight ratio, non-melting
- Good dimensional stability, including excellent thermal resistance
- Pigmentable for molded-in color; best appearance with mold texture
- Excellent property retention in cold and hot environments
- Good corrosion resistance except in acid environments.
- Designed for compression molding in matched metal die molds.
A. Schulman has acquired this former Premix product line. |