MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ITW Plexus Plexus™ MA420FS Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.

All purpose adhesive, very fast curing.

Information provided by Illinois Tool Works.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.977 g/cc0.0353 lb/in³Mixed
Viscosity 50000 - 80000 cP50000 - 80000 cPB
 80000 - 100000 cP80000 - 100000 cPA
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 8.62 - 10.3 MPa1250 - 1500 psi
Elongation at Break 5.0 - 15 %5.0 - 15 %
Tensile Modulus 0.241 - 0.345 GPa35.0 - 50.0 ksi
Shear Strength 8.96 - 11.0 MPa1300 - 1600 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point 10.6 °C51.0 °FTCC
 
Processing PropertiesMetricEnglishComments
Pot Life 1.0 - 2.0 min1.0 - 2.0 min
 
Descriptive Properties
ColorOff-white
Fixture Time3-4 minutes
Gap FillingMax 0.125 in
Mix Ratio10:1By volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 919 Epoxy Prepreg with Kevlar 49 Aramid Fiber, Weave Style 285
Röchling GoldMember™ Pre-tensioned Fiber Reinforcements
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, Hybrid carbon/Aramid fabric 245 g/m2
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Overview of materials for Ethylene Butyl Acrylate

PMM9006 / 53314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.