Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature to a tough, flexible to semi-rigid polymer depending upon the mix ratio employed. It has good wetting and adhesion to most surfaces and has a free flowing viscosity. It has very good resistance to water, acids and bases and most organic solvents. It was especially formulated to allow users to vary mix ratio to achieve desired hardness and flexibility. It can be mixed anywhere from an A/B ratio of 2 to1 to 1 to 2 by weight or volume. EP1215 will normally reach full cure at room temperature within 24 –48 hours. Cure time can be accelerated by the application of heat. Times and temperatures from 2 hours at 65°C to 10 minutes at 100°C are typical for most applications. Time to heat substrate must be taken into account. Cooler temperatures will also extend work time and increase cure times.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company. |