MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

3D Systems LaserForm® AlSi12 (B), AS-BUILT Aluminum Alloy Material
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: LaserForm AlSi12 (B) is formulated and fine-tuned specifically for 3D Systems’ ProX® DMP 200 and 300 metal 3D printers to deliver highest part quality and best part properties.

Known for its high strength–to-weight ratio and good thermal properties, the lightweight Laserform AlSi12 (B) is frequently used in aerospace, aviation, motorsports and automotive applications as well as for specifically thin-walled applications such as the production of heat exchangers. With Direct Metal Printing, parts that were typically cast are now being directly printed. Even more complex designs than typical casting processes allow can be produced in one single piece using DMP.

Classification: The chemical composition of LaserForm AlSi12 (B) conforms to the requirements of ISO 18273, ISO 17672, UNS A94047 and DIN EN 1706 specifications.

Information provided by 3D Systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.685 g/cc0.09700 lb/in³Absolute theoretical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 84 - 11084 - 110ISO 6506-1
Tensile Strength, Ultimate 440 - 500 MPa63800 - 72500 psiHorizontal direction — XY; ASTM E8M
 480 - 500 MPa69600 - 72500 psiVertical direction — Z; ASTM E8M
Tensile Strength, Yield 250 - 270 MPa36300 - 39200 psiRp0.2%, Vertical direction - Z; ASTM E8M
 270 - 310 MPa39200 - 45000 psiRp0.2%, Horizontal direction - XY; ASTM E8M
Elongation at Break 4.0 - 8.0 %4.0 - 8.0 %Vertical direction — Z; ASTM E8M
 6.0 - 10 %6.0 - 10 %Horizontal direction — XY; ASTM E8M
Tensile Modulus 6.00 - 7.00 GPa870 - 1020 ksiYoung's, Vertical direction — Z
 6.50 - 7.50 GPa943 - 1090 ksiYoung's, Horizontal direction — XY
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000450 - 0.00000620 ohm-cm0.00000450 - 0.00000620 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 - 600 °C
11.1 µin/in-°F
@Temperature 68.0 - 1110 °F
Thermal Conductivity 130 - 150 W/m-K
@Temperature 50.0 °C
902 - 1040 BTU-in/hr-ft²-°F
@Temperature 122 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 86.4 - 89 %86.4 - 89 %
Nitrogen, N <= 11 %<= 11 %
Silicon, Si <= 13 %<= 13 %
 
Descriptive Properties
Element<0.6Residuals

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems LaserForm® AlSi12 (B), STRESS RELIEF Aluminum Alloy Material
Erbslöh Aluminium DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7
Erbslöh Aluminium DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6
Erbslöh Aluminium DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6
Aluminum 413.0-F Die Casting Alloy

PAPPR3167 / 239135

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.