Heat Treatment Condition T7 (Quenching in water at RT) Excellent properties: - abrasive stability
- high stiffness (E-modulus)
- resistance even at high temperatures
- good grindability
PEAK DISPAL materials allow the manufacturing of pistons for highest operational demands. Information provided by PEAK Werkstoff GmbH, a part of Erbslöh Aluminium GmbH. |