MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Sika SikaFlex® 221 Fast Cure Polyurethane Sealant/Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Sika 221 SikaFlex Fast Cure Polyurethane Sealant/Adhesive
This versatile product is the most popular adhesive/sealant. It is an excellent adhesive/sealant and can handle many light bonding applications. USDA and potable water approved. 10 mm Cut-Off. Available in black, white gray, tan, colonial white, designer beige. Good non-sag. Cure Type: Moisture

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0446 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 45 - 5045 - 50
Tensile Strength, Ultimate 1.55 MPa225 psi
Elongation at Break >= 600 %>= 600 %
Adhesive Bond Strength 1.14 MPa165 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 87.8 °C190 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourValue given per 1/8 inches
Tack-Free Time 60.0 - 120 min1.00 - 2.00 hour
Shelf Life 9.00 Month9.00 Month
 
Compliance PropertiesMetricEnglishComments
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sika SikaFlex® 201 Adhesive
Sika SikaFlex® 255FC Fast Cure One Part Polyurethane Adhesive
Dow 732 MULTI-PURPOSE SEALANT
Sika SikaFlex® 252 One Part Polyurethane Adhesive
Overview of materials for Epoxy Adhesive

PSIKA01 / 67719

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.